- Chemical Waste[4]
- Water Treatment[10]
- Ceramics[10]
- Other Filter Supplies[1]
- Aluminum Pipes[1]
- Valve Balls[3]
- Ceramic Ball Bearing[1]
- Bearing Balls[1]
- Other Environmental Products[1]
- Reactors[2]
- Other Non-Metallic Mineral Deposit[2]
- Catalyst[6]
- Kaolin[1]
- Other Mining Machinery[1]
- Other Lab Supplies[1]
- Refractory[2]
- Other Aluminum[1]
- Other Metals & Metal Products[4]
- Chemical Process Equipment Parts[4]
- Separation Equipment[1]
- Chemical Projects[1]
- Stainless Steel Scrap[1]
- Other Air Cleaning Equipment[1]
- Pressure Vessels[1]
- Other Plastic Products[7]
- Other Inorganic Chemicals[1]
- Chemical Auxiliary Agent[9]
- PP[1]
- Other Petrochemical Related Products[1]
- Other Chemicals[1]
- Contact Person : Mr. Duan Wenhui
- Company Name : Jiangxi HH Petrochemical Packing Manufacture
- Tel : 86-799-3429235
- Fax : 086-0799-3429685
- Address : Jiangxi,Pingxiang,Lashi Industrial Zone
- Country/Region : China
- Zip : 337027
Activated ceramic ball
1.Performance characteristics
Activated ceramic ball is a new support material of catalyst. It added a small amount of transition metal oxide into the inert ceramic ball. It has the property of high-temperature resistance .high pressure and strength of the inert ceramic ball to filtrate. disperse vapor-liquid coverage and support the catalyst, In addition, it has adequate catalytic activity when used in the process of olefin hydrogenation desulfurization, denitrification to help catalysis.If been set on the top of catalysts bed in the reactor of distillates hydrotreating, hydrocracking, reforming pre-hydrogenation and hydrogenation of benzene hydrogenation, the activated ceramic ball make the olefin in the secondary processing fraction pre-hydrogenated and keep the catalyst from cokings. similarly, if been set on the bottom, it can remove the thio-alcohol caused in the reaction process. on the whole, using the activated ceramic ball can not only save the space in reactor, but also protect the catalyst from poisoning or sintering. consequently prolong the service life of catalyst.
2.Technical indicators
Type | Ni-Mo | Ni-W | Co-Mo | |
Active component | NiO 0.5-1.0MoO3 1.5-2.5 | NiO 0.5-1.0WO3 1.5-2.5 | CoO 0.5-1.0MoO3 1.5-2.5 | |
Appearance | Tawny | Pale yellow | Light grey | |
Pore volume,ml/g | 0.1-0.2 | |||
Heat-resistant temperature, | ≥800 | |||
Attrition rate,% | ≤5 | |||
Compressive strength N / particle | Φ3-10 | ≥150 | ||
Φ13-20 | ≥500 | |||
Φ25-50 | ≥1200 | |||
Φ75 | ≥3500 | |||
bulk density,kg/m³ | 1100-1300 | |||
Note:The data of bulk density is just for your reference only, not the standard for checking. |
3.Catalytic property
Model | Ni-Mo | Ni-W | Co-Mo | |||||
Reaction temperature,oC | 275 | 300 | 300 | 320 | 350 | 300 | 320 | 350 |
Hydrogen pressure,MPa | 3.0 | 3.0 | 3.0 | 3.0 | 3.0 | 3.0 | 3.0 | 3.0 |
Liquid space velocity,h-1 | 10 | 10 | 4.2 | 4.2 | 4.2 | 4.2 | 4.2 | 4.2 |
Ratio of hydrogen/oil | 600 | 600 | 450 | 450 | 450 | 450 | 450 | 450 |
Sulfur content,% | 2.5 | 2.5 | 2.5 | 2.5 | 2.5 | 2.5 | 2.5 | 2.5 |
Olefin content,% | 27.5 | 27.5 | 27.5 | 27.5 | 27.5 | 27.5 | 27.5 | 27.5 |
Rate of desulfation,% | 76 | 95 | 40 | 60 | 77 | 36 | 54 | 63 |
Olefin saturation,% | 68 | 95 | 10 | 33 | 45 | 7 | 19 | 42 |
4.Size
Diameter,Φ | 3 | 6 | 8 | 10 | 13 | 16 | 20 | 25 | 30 | 38 | 50 | 75 |
Diameter tolerance,mm | ±1.0 | ±1.5 | ±2.0 | ±3.0 |